聚晶金刚石复合片及其生产工艺简述〔1〕聚晶金刚石复合片〔液〕压机上,承受先进的超高压-高温合成工艺,生产聚晶金刚石复合片坯料(1)Polycrystallinediamondcompact(PDC)Selectandusedomesticrawmaterials,andaftertheproceduresofre-coining,purification,purging,burdeningandassembling,useadvancedultrahighpressure-hightemperaturesynthesistechnologytoproducepolycrystallinediamondcompact(PDC)billetonthedomesticcubic(hydraulic)press.聚晶金刚石复合片具体生产工艺简述:1〕依据订单和公司打算下达生产任务单;原料、辅料的购置;规章外形的金刚石颗粒,获得圆度好的、根本上为球形的金刚石颗粒;Introductionofthespecificproductiontechnologyofpolycrystallinediamondcompact(PDC):Assignproductiontasksinaccordancewiththeordersandcompanyplan;Purchaserawmaterialsandauxiliarymaterials;Coining:strictlycontrolthediamondshape,re-cointhepurchasedrawmaterials,anddothebesttoeliminatethediamondparticleswithirregularshapessuchasstriponestoobtaindiamondparticleswithgoodroundnessandwhicharebasicallyspherical.时间不同的原理选取所需粒度,使用激光粒度对粒度的分布进展准确测量;5〕净化:对金刚石微粉、钴粉及其他原料进展氢气复原处理;氢气复原处理工艺:在氢气复原炉中处理,依据材料的不同选择不同的处理温度,大致范围500-800℃;Classification:putthemixedpowderintothebeaker,addsuper-purgativedeionizedwater,stirandmixitevenly,selectrequiredparticlesizeinaccordancewiththesettlingtimetheoryofdifferentparticlesizes,andusethelaserparticlesizeanalyzertoaccuratelymeasurethedistributionofparticlesizes;Purification:performhydrogenreductivetreatmenttodiamondmicro-powder,cobaltpowderandotherrawmaterials;hydrogenreductivetreatmenttechniques:processitinthehydrogenreducingfurnace,selectdifferenttreatmenttemperaturesinaccordancewithdifferentmaterials,andtheproximaterangeshouldbebetween500-800℃;度严格把握,强调平均粒度以及不同粒度的协作比例。所配原料Co等原料,改为适宜的粘结剂粉末〔铝、氮化铝、氮化钛等各种粉末;Burdening:mixthediamond,cobaltpowdeandasmallamounofmicroelementsinaccordancewithacertainproportion,ofwhichthediamondparticlesizesshouldbeunderstrictcontrol,andthemixtureratioofaverageparticlesizeanddifferentparticlesizesshouldbeemphasized.Adequatelymixtheburdenedrawmaterialsintheballmill,andstrictlycontroltheballmillingtimeandtherotatingspeedoftheballmill;whenloadingbig-sizepolycrystallinediamondcuttingblades,specialloadingmethodshouldbeadoptedtoensureeventhicknessofthepolycrystallinediamondlayerinthecompact;forthepolycrystallinecubicboronnitride(PCBN)cuttingblades,duringtheprocedure,changethediamondmicro-powderintomaterialslikeboronnitridemicro-powderandCo,andchangeitintoappropriatebinderpowder(suchasvariouspowderslikealuminium,aluminiumnitrideandtitaniumnitride).200t油压机上压制近似于立方体的叶蜡岩块10-3Pa的状况下进展真空热处理,冷却出炉后尽快将原料放入钼杯中并用钼盖盖好;。假设需要合成大尺寸的聚晶金刚石复合片,需选用大吨位的六面顶压机,针对局部产品及202301500-1800℃,压力最大保持6GPa。该步骤是整个工序中最重要的局部,也是技术的核心,必需优化工艺参数以到达最优化的合成工艺。产品种类、规格不同,合成所用参数需要调整;PCBN合成时,合成方法与合成聚晶金刚石刀片的方法一样,但工艺参数依据氮化硼含量和粘结剂含量、种类的不同而有较大的不同。Assembling:pressthepyrophylliteblockswithcubicshapesonthe200toilhydraulicpress;performvacuumheattreatmenttotheballmilledmaterialsunderavacuumdegreeof10-3Pa,putthematerialintothemolybdenumcupassoonaspossibleafterdischargeandcooling,andcoveritwellwithamolybdenumcap;Synthesis:chooseacubicpressofappropriatetonnageinaccordancewiththesizeofPDCtoperformsuperhighpressure-hightemperaturesynthesis.Synthesisofbig-sizePDCrequirescubicpressofbigtonnage,andsometimesthecurrentbiggestdomesticcubicpressof20,000tonageisneededinaccordancewithspecialtechnologicalrequirementsofsomeproductsandprocedures.Requiredtemperatureis1500-1800℃,andthebiggestpressureis6GPa.Thisstepisthemostimportantpartinthewholeprocedureaswellascoreofthetechnology,andtechnologicalparametersmustbeoptimizedtogenerateoptimizedsynthesistechnology.Parametersusedinthesynthesisneedtobeadjustedinaccordancewithdifferentproductcategoriesandsizes;whensynthesizingPCBN,themethodisthesamewiththesynthesisofpolycrystallinediamondcuttingblades,buttherearemajordifferencesoftechnologicalparametersinaccordancewithdifferentcontentsandcategoriesofboronnitrideandbinder.,除去加工合成过程中和去除叶蜡岩块和钼杯时黏附的氧化物、叶蜡岩等,露出产品坯料;10〕磨外圆:对产品坯料用外圆磨床磨外圆。由于超高压高温合成过程中原料会发生流淌,同时,通过磨外圆把握样品的尺寸〔直径;Sandblast:thesynthesizedproductisinthepyrophylliteblock.Firstremovethepyrophylliteblockandcoveredmolybdenumcup,andthenperformsandblasttreatmenttoremoveadheredoxideandpyrophyllitefromthesynthesisprocessandremovalofthepyrophylliteblockandmolybdenumcuptoexposetheproductbillet;Externalgrinding:usethecylindricalgrindertoperformexternalgrindingtotheproductbillet.Becausethematerialmayhavefluctuatedduringthesuperhighpressure-hightemperaturesynthesis,sotheobtainedproductmaynothaveaperfectshapeandmeettherequirementofproductappearance,andaperfecylinderhastobeobtainedthroughexternalgrinding.Inthemeantime,externalgrindingcanalsobeusedtocontrolthesizethesample(diameter);研磨:主要承受电火花进展平面切削这一突破性工艺,以削减单纯研磨所造成的工序所需时间很长,所消耗的金刚石磨料量大的缺陷;当电火花切削产品坯料接近所需尺寸时,再承受高精度双面研磨机研磨到所需尺寸〔厚度;0.1-0.5mm,角度45;刀片可能需要依据用户要求分割为大小和外形不同的切割片Grinding:electricdischargemachine(EDM)ismainlyadoptedtoperformthebreakthroughtechnologyoffacecuttingtoovercomethedefectsoflongprocesstimeandbigamountofabrasivematerialsduringthepuregrinding;afterusingtheelectricdischargemachine(EDM)tocuttheproductbilletclosetotherequiredsize,thenusethehigh-precisiondouble-facedgrindingmachinetogrinditintotherequiredsize(thickness);Chamferofflatgrinding:thechamfershouldbeabout0.1-0.5mmwithanangleof45;thebladescanbedividedintocuttingbladesofdifferentsizesandshapesinaccordancewiththecustomerrequirement;〔包括尺寸公差、平坦度、外表缺陷、机械损伤以及长时间存放时腐蚀程度分级,合格后装箱。这是保证产品质量的重要步骤;在成品检测过程中更强调聚晶金刚石的厚度的测定14〕包装装箱:出厂的产品外观、尺寸必需能到达国外同类著名公司产品同样的标准,同时要保证产品经长途运输〔特别是国外用户,产品外观、尺寸不会变化;15〕入库:经检验合格的产品须按不同品种、规格、等级等分门别类进展入库储存。Productinspection:inaccordancewithtechnicalrequirementsofthecompanyandcustomer,inspectionofitemssuchasappearance,dimensions(includingdimensionaltolerances,flatness,surfacedefect,mechanicaldamageandcorrosivede

温馨提示

  • 1. 本站所有资源如无特殊说明,都需要本地电脑安装OFFICE2007和PDF阅读器。图纸软件为CAD,CAXA,PROE,UG,SolidWorks等.压缩文件请下载最新的WinRAR软件解压。
  • 2. 本站的文档不包含任何第三方提供的附件图纸等,如果需要附件,请联系上传者。文件的所有权益归上传用户所有。
  • 3. 本站RAR压缩包中若带图纸,网页内容里面会有图纸预览,若没有图纸预览就没有图纸。
  • 4. 未经权益所有人同意不得将文件中的内容挪作商业或盈利用途。
  • 5. 人人文库网仅提供信息存储空间,仅对用户上传内容的表现方式做保护处理,对用户上传分享的文档内容本身不做任何修改或编辑,并不能对任何下载内容负责。
  • 6. 下载文件中如有侵权或不适当内容,请与我们联系,我们立即纠正。
  • 7. 本站不保证下载资源的准确性、安全性和完整性, 同时也不承担用户因使用这些下载资源对自己和他人造成任何形式的伤害或损失。

评论

0/150

提交评论