耐热铸钢和热强铸钢德国标准DIN 174651993发布时间:2008-1-21 15:23:43 来源:中国压铸网德国DIN标准铁素体热强铸钢DIN 172451987铁素体热强铸钢的钢号与化学成分(质量分数)(%)钢 号材料号CSiMnPSCrNi其他GS-C251.061901.80.230.300.600.500.800.0200.0150.30GS-22Mo41.54190.180.230.300.600.500.800.0200.0150.30Mo0.350.45GS-17CrMo5 51.73570.150.200.300.600.500.800.0200.0151.001.50Mo0.450.55GS-18CrMo9 101.73790.150.200.300.600.500.800.0200.0152.002.50Mo0.901.10GS-17CrMoV5 111.77090.150.200.300.600.500.800.0200.0151.201.50Mo0.901.10V0.200.30G-XCrNi121.41070.060.100.100.400.500.800.0300.02011.512.50.801.50Mo0.50N0.05G-XCrMoV12 11.49310.200.260.100.400.500.800.0300.02011.312.20.701.00Mo1.001.20V 0.250.35(W0.50)铁素体热强铸钢的力学性能钢 号材料号b/MPa下列温度时的0.2/MPa5=(%)AKV/J20oC200oC300oC350oC400oC450oC500oC550oCGS-C251.06194405902451751451351301252227GS-22Mo41.54194405902451901651551501451352227GS-17CrMo5 51.73574906403152552302152051901801602027GS-18CrMo9 101.73795907404003553453303153052802401840GS-17CrMoV5 111.77095907804403853653503353203002601527G-XCrNi121.41075406903552752652602551835G-XCrMoV12 11.49317408803854504304103903703402901521德国DIN标准耐热铸钢DIN 174651993耐热铸钢的钢号与化学成分(质量分数)(%)钢 号材料号CSiMnPSCrNi其他GX30CrSi61.47100.200.351.02.50.51.00.0350.0306.08.0GX40CrSi131.47290.300.451.02.50.5 1.00.0350.03012.014.0GX40CrSi171.17400.300.451.02.50.51.00.0350.03016.018.0GX40CrSi231.47450.300.451.02.50.51.00.0350.03022.024.0GX40CrSi291.47760.300.451.02.50.51.00.0350.03027.030.0GX130CrSi291.47771.201.401.02.50.51.00.0350.03027.030.0GX40CrNiSi27-41.48230.350.501.02.51.50.0350.03025.028.03.55.5GX25CrNiSi18-91.48250.150.301.02.51.50.0350.03017.019.08.010.0GX40CrNiSi22-91.48260.300.501.02.51.50.0350.03021.023.09.011.0GX25CrNiSi20-141.48320.150.301.02.51.50.0350.03019.021.013.015.0GX40CrNiSi25-121.48370.300.501.02.51.50.0350.03024.026.011.014.0GX40CrNiSi25-201.48480.300.501.02.51.50.0350.03024.026.019.021.0GX40CrNiSi38-181.48650.300.501.02.51.50.0350.03017.019.036.039.0GX40CrNiSi35-251.48570.300.501.02.51.50.0350.03024.026.034.036.0GX30CrNiSiNb24-241.48550.250.400.52.01.50.0350.03023.025.023.025.0Nb1.21.8GX40CrNiSiNb38-181.48490.300.501.02.51.50.0350.03017.019.036.039.0Nb1.21.8GX40CrNiSiNb35-251.48520.350.451.02.51.50.0350.03024.026.033.035.0Nb0.81.8G-CoCr282.47780.100.200.51.51.50.0350.03027.030.0Co18.052.0G-NiCr28W2.48790.350.500.52.01.50.0350.03027.030.047.050.0W4.05.5耐热铸钢的室温力学性能钢 号材料号铸钢件状态力学性能(不小于)硬 度HBS300.2/MPab/MPa5(%)铁素体形GX30CrSi61.4710800850oC退火300GX40CrSi131.4729300GX40CrSi171.1740300GX40CrSi23GX40CrSi29GX130CrSi291.47451.47761.4777铸态铁素体奥氏体型GX40CrNiSi27-41.4823铸态奥氏体型GX25CrNiSi18-91.4825铸态23044015GX40CrNiSi22-91.48262304408GX25CrNiSi20-141.483223044010GX40CrNiSi25-121.48372304407GX40CrNiSi25-201.48482304406GX40CrNiSi38-181.48652304005GX40CrNiSi35-251.48572304405GX30CrNiSiNb24-241.48552304405GX40CrNiSiNb38-181.48492204005GX40CrNiSiNb35-251.48522204005GCoCr282.4778GNiCr28W2.4879耐热铸钢的高温力学性能钢 号材料号下列温度时110000h的蠕变强度MPa最高工作温度/oC600oC700oC800oC900oC1000oC1100oCGX30CrSi6GX40CrSi13GX40CrSi17GX40CrSi23GX40CrSi29GX130CrSi291.47101.47291.17401.47451.47761.477719.52222262689911112.52.53.555111.51.5750850900105011501100GX40CrNiSi27-41.482321941.51100GX25CrNiSi18-9GX40CrNiSi22-9GX25CrNiSi20-14GX40CrNiSi25-12GX40CrNiSi25-201.48251.48261.48321.48371.4848788282444646506622232326369.5101012.5175.5790095095010501100GX40CrNiSi38-18GX40CrNiSi35-251.48651.485755703240

温馨提示

  • 1. 本站所有资源如无特殊说明,都需要本地电脑安装OFFICE2007和PDF阅读器。图纸软件为CAD,CAXA,PROE,UG,SolidWorks等.压缩文件请下载最新的WinRAR软件解压。
  • 2. 本站的文档不包含任何第三方提供的附件图纸等,如果需要附件,请联系上传者。文件的所有权益归上传用户所有。
  • 3. 本站RAR压缩包中若带图纸,网页内容里面会有图纸预览,若没有图纸预览就没有图纸。
  • 4. 未经权益所有人同意不得将文件中的内容挪作商业或盈利用途。
  • 5. 人人文库网仅提供信息存储空间,仅对用户上传内容的表现方式做保护处理,对用户上传分享的文档内容本身不做任何修改或编辑,并不能对任何下载内容负责。
  • 6. 下载文件中如有侵权或不适当内容,请与我们联系,我们立即纠正。
  • 7. 本站不保证下载资源的准确性、安全性和完整性, 同时也不承担用户因使用这些下载资源对自己和他人造成任何形式的伤害或损失。

评论

0/150

提交评论